Pragati Marine plywood is manufactured from durable face and core veneers, so it performs longer in both humid and wet conditions and resists delaminating and fungal attack. Its construction is such that it can be used in environments where it is exposed to moisture for long periods.
The finished plywood is subjected to proper chemical treatment with Water-Soluble fixed type preservatives under vacuum pressure to ensure protection against wood destroying organism and to make the product insects, borer, termites and fungi free.
Thickness | : | 4,   6,   9,   12,   16,   18,   22,   25 mm |
|
Test |
ISI Requirements |
Observed Values |
1 |
Grade |
BWR,MR |
BWR |
2 |
Moisture Content |
5-15% |
7% |
3 |
Density |
0.65 to 0.70 gm/cm3 |
0.70 gm/cm3 |
4 |
Resistance to Water (3 cycles of hr Boiling & |
Min Pass |
Excellent |
5 |
Resistance to Micro Organism-Adhesion to plies |
Min Pass |
Excellent |
A |
Modulus of Elasticity -Along the Grain -Across the Grain |
Avg. Min 5000N/mm2 Avg. Min 2500N/mm2
|
7500N/mm2 4000N/mm2 |
B |
Modulus of Rupture -Along the Grain -Across the Grain |
Avg. Min 40 N/mm2 Avg. Min 20 N/mm2
|
60 N/mm2 35 N/mm2 |
6 |
Tensile Strength - Along the Grain - Across the Grain - Sum of Tensile Strength |
Avg. Min 42.00 N/mm2 Avg. Min 25.00 N/mm2 Avg. Min 84.50 N/mm2
|
52 N/mm2 38 N/mm2 90 N/mm2 |